+86 731 8411 3962
Ronsco is a leading supplier of superalloy in China, enowned for our exceptional production standards, strict quality control, extensive inventory, and unwavering commitment to excellence. We specialize in supplying superalloy tube & pipe in various OD, ID, wall thickness and length, to meet customers' needs for different projects.
|
Sizes |
Range |
|
Outside Diameter |
3.175-219.1 mm |
|
Wall Thickness |
0.5-12.7 mm |
In addition to on-demand production, we also offer an large inventory, regularly stock a variety of materials and specifications. Regardless of project size, we can all meet deadlines and deliver final products that meet or exceed industry standards.
As an superalloy supplier with over 28 years of experience, our product range is extensive, covering a variety of materials, particularly in Nimonic 80A, Nimonic 75 etc., to meet the needs of various industrial fields.
|
Grades |
UNS |
EN |
GB |
|
Nimonic 80A |
N07080 |
2.4631/2.4952 |
GH3039 |
|
Nimonic 75 |
N06075 |
2.4630/2.4951 |
GH3030 |
Are you looking for a reliable tubes manufacturer? Ronsco will be your first choice. We always adheres to the business phiosophy of "customer-centered", tries its best to meet the requirements of customers and pursues win-win cooperation with customers. Please provide the follow information to request a latest quotation now! Email: manager@ronsteel.com
|
No |
Information |
|
1 |
Name |
|
2 |
Standard And Grade |
|
3 |
Size |
|
4 |
Quantity Or Weight |
|
5 |
Process, Surface And Any Special Requirements etc. |
Superalloys tube & pipe is a special category of advanced materials, the unique feature of this alloy lies in their ability to maintain their mechanical properties at elevated temperatures, where conventional materials would typically degrade. The dual-phase microstructure of superalloys, similar to duplex tube, allows them to offer a unique combination of strength, ductility, and toughness, maintain structural integrity under challenging conditions. Furrthermore, it also offers oxidation resistance and creep resistance. These properties make it ideal for the aerospace filed etc, excel in withstanding harsh environments and demanding operating conditions.



Pure nickel tube & pipe composed entirely of nickel, the purity of nickel ensures a high level of corrosion resistance, making them ideal for environments where protection against corrosion is paramount.
| Grades | UNS | EN | GB |
| Nickel 200 | N02200 | 2.4060 / 2.4066 | N6 |
| Nickel 201 | N02201 | 2.4061 /2.4068 | N5 |

Nickel alloy tube & pipe is prized for their ability to excel in extreme conditions, the unique chemical composition and mechanical properties are different from traditional materials.
| Grades | UNS | EN | DIN |
| Inconel 600 | N06600 | 2.4816 | NiCr15Fe |
| Inconel 601 | N06601 | 2.4851 | NiCr23Fe |
| Inconel 617 | N06617 | 2.4663 | NiCr23Co12Mo |
| Inconel 625 | N06625 | 2.4856 | NiCr22Mo9Nb |
| Inconel 690 | N06690 | 2.4642 | NiCr29Fe |
| Inconel 718 | N07718 | 2.4668 | NiCr19NbMo |
| Inconel X-750 | N07750 | 2.4669 | NiCr15Fe7TiAl |
| Sanicro 28 | N08028 | 1.4563 | X1NiCrMoCu 31-27-4 |
| Incoloy 800 | N08800 | 1.4876 | X10NiCrAlTi 32-20 |
| Incoloy 800H | N08810 | 1.4958 | X5NiCrAlTi31-20 |
| Incoloy 800HT | N08811 | 1.4959 | X8NiCrAlTi32-21 |
| Incoloy 825 | N08825 | 2.4858 | NiCr21Mo |
| Monel 400 | N04400 | 2.4360 | NiCu30Fe |
| Monel K500 | N05500 | 2.4375 | Ni63Cu30Al3Fe2Mn1.5Ti0.5 |
| Hastelloy C276 | N10276 | 2.4819 | NiMo16Cr15W |
| Hastelloy C22 | N06022 | 2.4602 | NiCr21Mo13Fe4W3 |

Superalloys tube & pipe is a special category of advanced materials, the unique feature of this alloy lies in their ability to maintain their mechanical properties at elevated temperatures, where conventional materials would typically degrade.
| Grades | UNS | EN | GB |
| Nimonic 80A | N07080 | 2.4631 / 2.4952 | GH3039 |
| Nimonic 75 | N06075 | 2.4630 / 2.4951 | GH3030 |

Austenitic stainless tube & pipe are a prevalent type of stainless steel with high levels of chromium and nickel, these tubes exhibit remarkable corrosion resistance, particularly in acidic environments.
| Grades | UNS | EN | DIN |
| 316L | S31603 | 1.4404 | X2CrNiMo17-12-2 |
| 316L Mod | S31723 | 1.4435 | X2CrNiMo18-14-3 |
| 316LVM | S31673 | 1.4441 | X2CrNiMo18-15-3 |
| 310MoLN | S31050 | 1.4466 | X1CrNiMoN25-22-2 |

Duplex stainless tube & pipe represent a specialized category of stainless steel known for their dual- phase microstructure, combining both austenitic and ferritic phases.
| Grades | UNS | EN | DIN |
| 2205 | S32205 / S31803 | 1.4462 | X2CrNiMoN22-5-3 |
| 2507 | S32750 | 1.4410 | X2CrNiMoN25-7-4 |
| F55 | S32760 | 1.4501 | X2CrNiMoCuWN25-7-4 |
Feel free to contact us by submitting this form or use our email. Our sales representative will contact you within 24 hours. Thank you for your interest in our products.